08/20/2021
The Process:
All parts are sand blasted and/or hand sanded then washed with degreaser or aluminum cleaner. Then they are pre-cooked at 400 degrees to remove any oil or contaminants that may be in the pores of the metal. Finally, the powder coating is applied and baked at 400 degrees until cured.
The Results: